Electoless Nickel Plating

Electoless Nickel Plating

Production Line

Product Property

  • High Phosphorus ENP (10-12 wt%)
  • Hardness: non-heat treatment (HV350-450),after heat treatment (HV450-600)
  • Need surface roughening product
  • Al alloy-6061 T6
  • SUS304/ Low-carbon steel/ Invar
  • Showerhead & Inner channel
  • Anti-corrosion test pass
  • (22 days acid air & 24 hrs acid solution)
  • Bright electroless-nickel-plating
  • Thickness: 10-50 µm ± 5 µm
  • Low porosity: < 2%

Inspection Equipment

Technique Certification